A selection of abstracts of clinically relevant papers from other journals. The abstracts on this page have been chosen and edited by John R. Radford.
Abstract
Thermocycling reduced dramatically the shear bond strengths of those test specimens with a lithium disilicate intermediate glass-ceramic layer.
Log in or create a free account to read this content
Gain free access to this article, as well as selected content from this journal and more on nature.com
or
Rights and permissions
About this article
Cite this article
Improving shear bond strength between feldspathic porcelain and zirconia substructure with lithium disilicate glass-ceramic liner. Br Dent J 219, 530 (2015). https://doi.org/10.1038/sj.bdj.2015.918
Published:
Issue date:
DOI: https://doi.org/10.1038/sj.bdj.2015.918