Figure 2
From: Pressure-induced amorphous-to-amorphous configuration change in Ca-Al metallic glasses

The parameter, , of the main amorphous peak, which is related to the reduced volume of the sample V(P)/V(0), as a function of pressure for Ca100−xAlx (x = 20, 27.3 and 33.6 at.%) MGs.
Transitions are marked by arrows. Error bars for experimental data are given and some are smaller than the symbol size. The solid lines are guides to the eye.