Table 1 Average pore size, specific surface area and total pore volume of the Normal films and the TiO2 photo-electrode films with different acetylene-black concentrations
TiO2 photo-electrode films | Normal | 0.5 wt% | 1.5 wt% | 2.0 wt% |
|---|---|---|---|---|
Average Pore Size (nm) | 17.572 | 21.750 | 23.298 | 23.665 |
as,BET (m2g−1) | 42.364 | 39.352 | 36.382 | 33.089 |
Total pore volume(cm3g−1) | 0.186 | 0.196 | 0.212 | 0.196 |