Figure 7

The decay curves of the carbon nitride products syntherized via the thermal condensation of melamine at different temperatures for 2 h (λex = 280 nm).
The decay curves of the carbon nitride products syntherized via the thermal condensation of melamine at different temperatures for 2 h (λex = 280 nm).