Figure 1
From: Fatigue-Induced Damage in Zr-Based Bulk Metallic Glasses

A schematic diagram of the experimental design.
The as-cast sample undergoes compression-compression fatigue until it fails. Then, the damaged part is cut off and the leftover is used for the next fatigue test as long as the rest part has an L/D ratio greater than 0.8.