Table 2 Volumes and fatigue lives of ten experimental specimens
From: Fatigue-Induced Damage in Zr-Based Bulk Metallic Glasses
Sample, i | Volume, Vi(mm3) | Cycles to failure, Ni (million cycles) |
|---|---|---|
1 | 282.7433 | 0.484017 |
2 | 282.7433 | 0.552864 |
3 | 707.4238 | 1.535442 |
4 | 704.0309 | 0.304354 |
5 | 704.0309 | 1.315717 |
6 | 139.1097 | 1.26922 |
7 | 268.0407 | 3.00371 |
8 | 495.3663 | 1.70379 |
9 | 240.8973 | 2.10075 |
10 | 419.0256 | 4.63925 |