Table 1 Charge and discharge time for Co(OH)2/GNS electrode in 1 M KOH containing different concentrations of K3Fe(CN)6 mixed solution, calculated from galvanostatic charge-discharge curves at a current density of 16 Ag−1
From: Ultrahigh capacitive performance from both Co(OH)2/graphene electrode and K3Fe(CN)6 electrolyte
Concentration (M) | Charge time (s) | Discharge time (s) |
---|---|---|
0.01 | 28.2 | 29.3 |
0.02 | 29.9 | 37.6 |
0.04 | 51.1 | 83.7 |
0.06 | 60.0 | 171.3 |
0.08 | 52.7 | 285.3 |