Table 1 Dielectric Properties of BSTO and Mn:BSTO thin films on (001) MgO measured at 300 K and 2 GHz
From: The Origin of Local Strain in Highly Epitaxial Oxide Thin Films
Mn:BSTO Films on (001) MgO | BSTO Films on (001) MgO | ||||||
---|---|---|---|---|---|---|---|
Sample Types | Residual Match Strain | εr (0 V) | εr (40 V) | εr Tuning % | εr (0 V) | εr (40 V) | εr Tuning % |
(001)-0.0° off | 0 | 1480 | 755 | 49% | 1068 | 712 | 33% |
(001)-1.0° off | 0.014 | 1664 | 800 | 52% | 1028 | 682 | 34% |
(001)-3.0° off | 0.017 | 1059 | 663 | 37% | 790 | 598 | 24% |
(001)-5.0° off | 0.010 | 1655 | 635 | 62% | 1202 | 790 | 34% |