From: One-Step to Prepare Self-Organized Nanoporous NiO/TiO2 Layers and its Use in Non-Enzymatic Glucose Sensing

Figure 2

(A) Cyclic voltammograms of as-formed NiO/TiO2 nanostructures in 0.1 M NaOH, the samples were anodized at room temperature (curve a), 10°C (curve b) and 0°C (curve c). (B) The influence of ultrasonicated time in H2O2 on the anodic peak currents of NiO/TiO2 layers. (C) Cyclic voltammograms of NiO/TiO2 layers in 0.1 M NaOH before (curve a) and after (curve b) ultrasonicated for 20 min in 30% H2O2. Scan rate: 50 mV s−1.