Figure 1
From: Disorder-induced Room Temperature Ferromagnetism in Glassy Chromites

Structural analysis.
(a) Using Focused Ion-Beam assisted Scanning Electron Microscope; thickness of film was determined to be around 435.6 nm; (inset) TEM diffraction pattern of thin film shows a halo indicating complete amorphization. (b) XRD of YCrO3 powder and pellet (used as target) shows orthorhombic crystal structure while the experimental radial distribution function for the thin film indicates only an amorphous phase on the silicon substrate.