Table 4 Cr(VI) removal efficiency and electrical parameters under different electrolytes

From: Remediation of chromium-slag leakage with electricity cogeneration via a urea-Cr(VI) cell

Systema

C0-Cr(VI) mM

OCP(V)

Cr(VI) removal efficiency

Total generation electricity (C)

Theoretical generation electricity (C)

Cathodic efficiency (%)

Urea + PBS-Cr(VI) t3

2.68

1.19

96.5%

-

-

-

Urea + KOH-Cr(VI) t1

1.34

1.56

96.7%

8.42

3.88

46.1

Urea + KOH-Cr(VI) t2

2.68

1.59

98.6%

11.3

7.76

68.6

Urea + KOH-Cr(VI) t3

5.35

1.59

98.6%

20.5

15.3

74.6

  1. at1 = 12 h, t2 = 18 h, t3 = 48 h.