Figure 3

PL decay process for emission peaks of the MQWs with different barrier thickness (samples D-F) at 8 K.
The obtained lifetimes τ1and τ2 are shown in place. It can be found τ2 dominates the process.
PL decay process for emission peaks of the MQWs with different barrier thickness (samples D-F) at 8 K.