Table 2 Characteristic parameters determined by model analysis of SAXS for aqueous suspensions of vermiculite with Cs+
From: Collective Structural Changes in Vermiculite Clay Suspensions Induced by Cesium Ions
Sample No. | R (Å) | σR (Å) | N | f 1 | f 2 | D1 (Å) | D2 (Å) | σT,1 (Å) | σT,2 (Å) | σD,1 (Å) | σD,2 (Å) |
|---|---|---|---|---|---|---|---|---|---|---|---|
1 | 168 ± 4.4 | 33.1 ± 2.9 | 90.4 ± 14.3 | 0.73 | 0.27 | 14.9 ± 0.1 | 33.5 ± 0.5 | 0.44 ± 0.07 | 5.97 ± 0.72 | 4.37 ± 0.04 | 11.5 ± 0.4 |
2 | 164 ± 4.5 | 28.7 ± 2.6 | 98.8 ± 20.4 | 1 | 0 | 14.9 ± 0.1 | – | 0.50 ± 0.07 | – | 3.25 ± 0.04 | – |
3 | 169 ± 4.3 | 31.5 ± 2.3 | 91.8 ± 16.4 | 1 | 0 | 14.9 ± 0.1 | – | 0.44 ± 0.09 | – | 3.37 ± 0.04 | – |
4 | 166 ± 4.5 | 25.5 ± 2.7 | 53.7 ± 7.9 | 0.79 | 0.21 | 14.7 ± 0.1 | 14.0 ± 0.2 | 0.55 ± 0.08 | 1.50 ± 0.10 | 4.03 ± 0.05 | 0.54 ± 0.1 |
5 | 165 ± 8.1 | 83.1 ± 4.8 | 25.5 ± 3.5 | 1 | 0 | 12.6 ± 0.3 | – | 1.66 ± 0.25 | – | 4.48 ± 0.10 | – |