Figure 1

In situ XRD patterns of Li0.33Ni0.8Co0.15Al0.05O2 cathode material when heated from 25°C to 300°C in the absence of electrolyte.
In situ XRD patterns of Li0.33Ni0.8Co0.15Al0.05O2 cathode material when heated from 25°C to 300°C in the absence of electrolyte.