Figure 11

The XRD patterns of pristine VO2 film and VO2-SiO2 composite film (Si/V molar ratio = 0.8) after depositing in air for 6 months.
(a) VO2 film; (b) VO2-SiO2 composite film (Si/V molar ratio = 0.8).
The XRD patterns of pristine VO2 film and VO2-SiO2 composite film (Si/V molar ratio = 0.8) after depositing in air for 6 months.