Table 1 Mean biaxial flexural strength (MPa) and standard deviation for the two commercial glass ionomer cements. Similar letters do not indicate significant differences (Tukey HSD post hoc test, p < 0.05)
From: How mobile are protons in the structure of dental glass ionomer cements?
 | Biaxial flexural strength (MPa) | ||
---|---|---|---|
Material | 24 h | 7 days | 32 days |
Poly (VOCO Ionofil Molar AC) | 66 ± 6bc | 76 ± 7ab | 84 ± 13a |
Aqua (Aqua Ionofil Plus) | 54 ± 4cd | 52 ± 5cd | 49 ± 9d |