Table 1 Tensile test results for the W–Y2O3 alloy at different temperatures.

From: Mechanical properties and microstructural change of W–Y2O3 alloy under helium irradiation

Temperature

Yield strength δ 0.2 (MPa)

Tensile strength (MPa)

Elongation (%)

Elastic modulus

400

397.4

436

6.4

6.65

600

273.1

346

7.1

5.0

800

206.4

249

3.9

4.5