Table 2 Microhardness of the W–Y2O3 alloy.
From: Mechanical properties and microstructural change of W–Y2O3 alloy under helium irradiation
Areas | Non-irradiated area | Irradiated region | RS-irradiated area | Affected area |
---|---|---|---|---|
Hv, MPa | 338.4 | 288.5 | 330.4 | 328.1–365.8 |