Figure 4

Cyclic voltammetry curves of LiNi0.5Mn1.5O4 with different microstructures before and after 200 cycles at a rate of 2 C.
Cyclic voltammetry curves of LiNi0.5Mn1.5O4 with different microstructures before and after 200 cycles at a rate of 2 C.