Figure 4

Out of plane X-ray diffraction scans of p-DTS(FBTTh2)2:PC71BM blends.
2θ = 3.98°, 7.88° and 11.90°. With thermal annealing, the intensity of the peaks is enhanced. Addition of 0.25 vol% DIO generated broader peak with higher intensities.