Figure 5
From: Reference of Temperature and Time during tempering process for non-stoichiometric FTO films

Variation of [O]/[Sn] ratio along the depth of FTO films tempered at different conditions (a) tempered for 220 s at different temperatures (b) tempered at 700 °C for different time.