Figure 4
From: Crystallization and precipitation of phosphate from swine wastewater by magnesium metal corrosion

Effect of the G:M mass ratio on the solution pH and the PT recovery efficiency (Mg metal dosage, 10 g L–1; airflow rate, 1 L min–1).