Figure 3 | Scientific Reports

Figure 3

From: Investigation of the dynamic bending properties of MoS2 thin films by interference colours

Figure 3

Images of the MoS2 thin films with coloured interference fringes on the surface under a microscope after preservation for different times: (a) 1 hour, (b) 15 days and (c) 40 days.

(d) The height distribution curves with each height value calculated based on the red horizontal reference line in (a–c) and the fitting angles at the opening of the wedge-shaped gap are marked at the bottom of the curves.