Figure 2
From: Magnetic phase separation in double layer ruthenates Ca3(Ru1−xTix)2O7

Magnetic susceptibility vs. temperature measured with zero field cooling (ZFC) histories under an external field of 5000 Oe applied along a and b axes for
(a) Ca3Ru2O7; (b) x = 0.02; (c) x = 0.03; (d) x = 0.04 and (e) x = 0.05.