Figure 6
From: Vertical La0.7Ca0.3MnO3 nanorods tailored by high magnetic field assisted pulsed laser deposition

Temperature dependence of resistivity in the LCMO films measured at HM = 0 and 3 T, respectively.
The inset shows temperature dependence of MR in the LCMO films under HM = 3 T.