Figure 7
From: Vertical La0.7Ca0.3MnO3 nanorods tailored by high magnetic field assisted pulsed laser deposition

Magnetic field dependence of MR in the LCMO films at
(a) 100, (b) 150 and (c) 230 K, respectively.
From: Vertical La0.7Ca0.3MnO3 nanorods tailored by high magnetic field assisted pulsed laser deposition
Magnetic field dependence of MR in the LCMO films at
(a) 100, (b) 150 and (c) 230 K, respectively.