Figure 4

Compositional depth profile by XPS of the PZT thin film prepared from the Seeded Photosensitive solution at 400 °C.
(a) Photoelectron peak intensities of constituent elements of the sample during depth profiling. (b) Evolution of the C 1s core level signal as a function of depth and binding energy.