Figure 3 | Scientific Reports

Figure 3

From: Macroscopic tensile plasticity by scalarizating stress distribution in bulk metallic glass

Figure 3

SEM images of the tensile fracture features for as-cast and LSTT samples.

(a) Macroscopic fracture surface in the lateral surface. The double arrowed lines indicate the fracture angles. (b) Macroscopic feature of fracture surfaces in the cross-sectional view. (c) A series of high magnitude SEM images showing the typical microscopic fracture morphology corresponding to the parts marked by the green dashed circles in (b). The inserted picture gives the magnified graph of the marked part in the last picture of (c) and the typical size of the cone-shaped structure.