Figure 2 | Scientific Reports

Figure 2

From: Universal limiting shape of worn profile under multiple-mode fretting conditions: theory and experimental evidence

Figure 2

(a) The cross section of spherical indenter worn profile obtained experimentally due to torsional fretting wear at four consecutive time moments. Note the difference of vertical and horizontal scaling. The theoretical limiting worn shape calculated according to Eq. (3) for the same parameters as in experiment is shown by dashed curve. (b) The photo of the experimental indenter in the final state.