Figure 3
From: Phase transformation and deformation behavior of NiTi-Nb eutectic joined NiTi wires

TEM micrographs in the interfaces of brazed region sintered at 1180 °C for 4 min: (a) schematic illustrations of the studied areas for the following images, (b) dislocations combined martensite nucleation, (c) coarse martensite with SAED pattern in region D (inset), (d) rounded Ti2Ni and (e) TiC particles surrounded by acicular martensite.