Figure 2: The average particle size vs annealing temperature profile of the OLCs.

From: Inherently-Forced Tensile Strain in Nanodiamond-Derived Onion-like Carbon: Consequences in Defect-Induced Electrochemical Activation

Figure 2

10~20 HR-TEM pictures were taken for each OLC sample, from which 50–55 clearly isolated particles (See Fig. S4) were selected for the particle size measurement for each OLC sample. See Fig. S5 where the particle size distributions of each OLC samples were given.