Figure 4
From: Microstructure and mechanical behavior of metallic glass fiber-reinforced Al alloy matrix composites

TEM microstructure of the spark plasma sintered composite.
(a) Bright–field TEM image. (b) HRTEM image of the interface between the metallic glass and the fcc-Al matrix. (c) SADF of the area corresponding to (a) indicating nanocrsytalline fcc-Al and amorphous structure. (d) SADF of the area 1 in (a) indicating amorphous structure. (e) SADF of the area 2 in (a) indicating fcc-Al structure. (f) SADF of the precipitate phase indicating the η-MgZn2 structure.