Figure 2

XRD patterns of uncoated LiMn1.5Ni0.5O4 particles and coated with different cycles of ALD iron oxide.
* indicates the dominant Fe3O4 phase due to iron oxide ALD coating.
XRD patterns of uncoated LiMn1.5Ni0.5O4 particles and coated with different cycles of ALD iron oxide.
* indicates the dominant Fe3O4 phase due to iron oxide ALD coating.