Figure 3

Bright-field TEM images of (a) LCMO:30%-NiO and (b) LCMO:30%-Co3O4 films grown on LAO substrates; cross-sectional high resolution TEM images of (c) LCMO:30%-NiO with inset image for NiO epitaxially grown with respect to LCMO matrix; and (d) LCMO:30%-Co3O4 on LAO substrates. The insets are the corresponding SAED patterns for each film (Yellow represents LCMO and LCMO-Co3O4, White represents LAO, and green represent NiO).