Table 1 Summary of parameters of LCMO:NiO and LCMO:Co3O4 composite films prepared from PAD method.

From: Enhancement of Low-field Magnetoresistance in Self-Assembled Epitaxial La0.67Ca0.33MnO3:NiO and La0.67Ca0.33MnO3:Co3O4 Composite Films via Polymer-Assisted Deposition

Sample

Out-of-plane lattice parameter [Å]

T P [K]

ρ [Ω•cm]

MR [%]

T C [K]

LCMO

3.858

270

0.0061

−44.6

10% NiO

3.897

180

0.59

−59.1

158

30% NiO

3.891

−31.7

144

10% Co3O4

3.898

172

1.07

−52.7

164

30% Co3O4

3.909

265

7.25

−43.4

210