Figure 4: The formation of a core-shell structure is robust across a wide range of ATPS compositions. | Scientific Reports

Figure 4: The formation of a core-shell structure is robust across a wide range of ATPS compositions.

From: Aqueous Two Phase System Assisted Self-Assembled PLGA Microparticles

Figure 4

(A) Partlcle morphology at 2% Pluronic F127/10% dextran, and PLGA concentration of 0.0625%. (B) Here the PLGA concentration is held at 0.0625%, but the concentration of Pluronic F127 and dextran are varied as follows. (B) (i) 2% Pluronic F127/10% dextran (ii) 5% Pluronic F127/10% dextran (iii) 5% Pluronic F127/5% dextran ATPS compositions. Scale bar 10 μm.