Figure 3
From: Selective Deposition of SiO2 on Ion Conductive Area of Soda-lime Glass Surface

AFM view of the glass surface after the electrical imprinting applying +200 V using the mold B, followed by the corona discharge in air containing cyclic siloxane vapor for 30 min at 200 °C.