From: Origin of Shear Stability and Compressive Ductility Enhancement of Metallic Glasses by Metal Coating

Figure 5

Deformation morphology for as-cast and coated MGs (Vit105, D = 2 mm).

(a) The SEM micrographs showing the side view for the as-cast sample and the coated sample (the right) after final failure. (b) An enlarged view around the shear step for the coated sample, showing the cracking of coating layer and the interface debonding. (c) An enlarged view on the region of debonding, showing features for severe plastic deformation of the coating layer.