Figure 3
From: Zinc Oxide Nanorods Shielded with an Ultrathin Nickel Layer: Tailoring of Physical Properties

Variation of the FWHM and dislocation density (DD) of ZnO and ZnO/Ni core/shell structures (S1-ZnO; S2-as-grown ZnO/Ni; S3-100 °C; S4-200 °C; S5-300 °C; and S6-400 °C annealed core/shell structures).