Figure 1

(a) HRTEM overview image of the Fe3O4/SrTiO3 heterostructure showing uniform film thickness of ~80 nm and a sharp interface between film and substrate. (b) SAD pattern from the interface region. The Fe3O4 and SrTiO3 motifs are outlined (Fe3O4 in red, SrTiO3 in green). (c,d) show SAD simulations of Fe3O4 (red) and SrTiO3 (green) depending on whether the Fe3O4 structure is mirrored around the vertical axis. (c) SAD along the [−110] viewing direction for both SrTiO3 and Fe3O4. (d) SAD along the [−110] viewing direction for SrTiO3 and the [1−10] viewing direction for Fe3O4. The correspondence between (b,d) shows that the Fe3O4 is mirrored from direct cube on cube epitaxy.