Figure 7: Variation of coercivity (Hc) and saturation magnetization (Ms) with different substrate temperature (Ts) of CoFe2O4 thin film. | Scientific Reports

Figure 7: Variation of coercivity (Hc) and saturation magnetization (Ms) with different substrate temperature (Ts) of CoFe2O4 thin film.

From: Switching of magnetic easy-axis using crystal orientation for large perpendicular coercivity in CoFe2O4 thin film

Figure 7

The magnetization measurements were carried out in ‘perpendicular’ and ‘In-plane’ directions of the film surface. Yellow pillar region in the Ms, and ‘Hc’ graphs denotes the magnetic measurements of randomly oriented CFO thin film. Ms values are considered to be remain unchanged for both ‘perpendicular’ and ‘In-plane’ directions.