Table 1 Data summarizing load vs. strain measurements of BHCNTs and control CNTs.

From: Boron-Filled Hybrid Carbon Nanotubes

Material

Fail Loading at Room Temp

Fail Temp at 30 μN

Stiffness in comparison to CNT

BHCNT-Outer Layer

75 μN

200 °C

130%

BHCNT-Inner Boron Wire

100 μN

400 °C

NA

CNT

30 μN

Room Temp

100%

CNT-COOH

50 μN (30 nm depth pen.)

200 °C

110%