Table 2 Combination of temperature and plastic strain tests.

From: Influence of low-temperature nitriding on the strain-induced martensite and laser-quenched austenite in a magnetic encoder made from 304L stainless steel

Group of samples

Engineering plastic strain applied in a single pass εd (%)

Pass 1

Pass 2

Pass 3

Pass 4

Pass 5

Pass 6

Pass 7

Pass 8

Pass 9

Pass 10

Pass 11

C−196°C

13.7

9.7

9.7

10.6

5.3

5.0

2.3

2.8

4.6

5.2

5.7