Figure 4

The quantity of protein absorption on four alloy samples after 4h of incubation in α-MEM medium containing 10% FBS.
Mg-1Ca-2.0Sr alloy absorbed more protein than other three alloy specimens and blank control, however, the differences were not significant (p > 0.05).