Figure 6
From: Unveiling the molecular mechanism of self-healing in a telechelic, supramolecular polymer network

Self-healing experiment.
(a) Schematic representation of the time dependence of strain and stress during the self-healing experiment. (b) Resulting normalized storage modulus during recovery for sample PIB14K-BA2 at different temperatures (25 °C, 20 °C, 15 °C, 10 °C, 5 °C) as a function of time t − t2.