Table 1 Comparison of the dielectric properties of our composites and reported literature materials at 100 Hz and room temperature.

From: Enhanced dielectric properties of poly(vinylidene fluoride) composites filled with nano iron oxide-deposited barium titanate hybrid particles

Composites

ε

tan δ

σ (S/cm)

f (vol.%)

Ref.

BT@Fe3O4/PVDF

138

0.24

1.4 × 10−9

40

Our work

BT@Fe3O4/PVDF#

385

0.3

4.12 × 10−9

33

Our work

BT@Fe3O4/PVDF#-1 kHz

280

0.27

2.50 × 10−8

33

Our work

Hydantoin/BT/P(VDF-HFP)

48.3

0.06

 

50

[12]

BT/PVDF treated by PVP

115

0.02

 

60

[27]

BT–Ag/PVDF-1 kHz

160

0.11

9 × 10−8

56.8

[17]

BT/SiC/PVDF

213.8

0.27

3.31 × 10−11

35

[28]

BT@SnO2/PVDF

≈160

≈1.35

≈1 × 10−8

45

[29]

R-ZnO/BT/PVDF

175

0.45

 

30

[30]

Ag@TiO2/PTFE

240

1

1 × 10−9

70

[31]

Al/β-SiCw/PVDF

350

0.48

 

52

[32]