Figure 2

Magnetization versus temperature measurements are shown for FC and ZFC for (a) bulk Dy and (b) a Dy thin film with a thickness of 42 nm measured for different in-plane fields. (c) Plot of furcation temperature TF versus field as obtained from the magnetization measurements shown in (a,b). The bulk was measured on PPMS while the thin film was measured on SQUID.