Figure 4
From: Kinetic ways of tailoring phases in high entropy alloys

Microstructures of annealed CoCrFeNiTi0.4 HEA; (a) 1080oC and quenching, (b) 1080oC and furnace cooling, (c) 900oC and quenching, (d) 900oC and furnace cooling.
From: Kinetic ways of tailoring phases in high entropy alloys

Microstructures of annealed CoCrFeNiTi0.4 HEA; (a) 1080oC and quenching, (b) 1080oC and furnace cooling, (c) 900oC and quenching, (d) 900oC and furnace cooling.