Figure 6

Cyclic voltammoram (CV) of ternary systems 0.025[LiTDI·y(glyme)]:0.975BMImTDI at room temperature containing (a). triglyme (y = 2.0 or 5.6), (b). tetraglyme (y = 2.0 or 4.5). Metallic lithium acts both counter and reference electrodes. The scan rate was 1 mVs−1.