Table 1 Raman shift of the diamond peak in relation to the substrate.

From: The pressure sensitivity of wrinkled B-doped nanocrystalline diamond membranes

Substrate

Diamond peak position (cm−1)

Diamond peak shift wrt single crystal diamond

Thermal expansion coefficient (°C−1)

Estimated Induced stress (GPa)

S-AF45 glass

1337.0 ± 0.5

5.3 ± 0.5

4.5 × 10−6 46

3.0 ± 0.3

CE2000 glass

1333.8 ± 0.3

2.1 ± 0.4

3.2 × 10−6 47

1.2 ± 0.2

Silicon

1333.9 ± 0.5

2.2 ± 0.5

2.6 × 10−6 48

1.2 ± 0.3

Single Crystal Diamond

1331.7 ± 0.2 49

/

1.0 × 10−6 50

/

  1. The peak position for single crystal diamond is shown as a reference.